2021-11-23
|
Features |
Causes |
Solutions |
Oxidation slag |
Oxidation slag distributes on the casting surface,in the stuffy corner parts of the mould.Fracture ashen white or yellow, It could be found by X-ray or during machining,can also be found in the alkaline cleaning, acid pickling or anodized. |
a.the furnace material is not clean and used material is overmch. |
a.Furnace material should be through blowing sand and appropriate reduce used material. |
Air hole |
Air hole inside casting wall is normally circular or elliptic with smooth surface,sometimes a yellow oil.Surface air hole could be found by sand blasting.Internal air hole have to be checked by X-RAY or machining. |
a.Casting alloy is not smooth, involved in gas |
a.Well control of casting speed and avoid gas. |
Shrinkage porosity |
Shrinkage of aluminum die castings is usually produced near thick parts of riser boots,large scale thin wall parts.Could be tested by X-ray,fluorescence macroscopic fracture,ect. |
a.Poor feeding function |
a.Add pouring metal liquid from the riser and improve the riser design. |
Crack |
a.Crack produced in casting process.Developed along the grain boundary, often accompanied by segregation, formed in a high temperature b.Crack produced in treat treatment process.Caused by heat treatment burnt or overheating. |
a.Casting structure design is unreasonable, there are sharp corners. |
a.Improve the design of casting,avoid sharp corners,try to keep wall thickness uniform when design. |